Abstract

The thermal degradation mechanisms of random copolymers of methacrylonitrile (MAN) and styrene (St) have been investigated by pyrolysis gas chromatography in the temperature range of 358 to 920‡C using a Curie point pyrolyzer (JHP-2) and comparing results with the results from TG/DTA-FTIR apparatus (SII-6200, JASCO-320). The amount of St monomer from decomposition of the copolymer is higher than that from P(St) alone; whilst that of MAN monomer from copolymer is lower than that from P(MAN). This phenomenon reflects the boundary effect in the pyrolysis of copolymer. The thermal degradation mechanisms of copolymers are discussed in terms of the competition between the depolymerization and the back biting reaction on the basis of bond dissociation energies of C-C and C-H bonds in the copolymer chain.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.