Abstract

Cubic boron nitride (cBN) particle-dispersed-aluminum (Al) matrix composites were fabricated from the powder mixture composed of cBN, pure Al and Al-5mass% Si alloy in liquid and solid co-existent state by spark plasma sintering (SPS) process. Al/cBN composites were well consolidated by heating at a temperature range between 798 K and 876 K for 1.56 ks by SPS. Microstructures of the composites produced were examined by scanning electron microscopy and the reaction between the cBN particle and the Al matrix was not detected. The relative packing density of the Al/cBN composite was higher than 99 % in a volume fraction range of cBN up to 45 %. The thermal conductivity of the composite increased with increasing the cBN content in the composite in a volume fraction range of cBN between 35 and 45 vol. %. The highest thermal conductivity of 305 W/mK was obtained for Al matrix composite containing 45 vol.% cBN particles.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call