Abstract
In recent years, the downscaling of transistors has sparked considerable interest in the advancement of amorphous oxide semiconductors, particularly indium-hafnium-zinc oxide (IHZO) has remarkable potential in applications such as high-resolution displays and 3D NAND. For the first time, we propose the fabrication of IHZO thin film transistors (TFTs) via thermal atomic layer deposition (TH-ALD). The preparation, electrical properties, and stability of IHZO TFTs are investigated. The performance of TFT deposited at 250 °C and annealed in N2 atmosphere at 300 °C exhibits a high field-effect mobility (μ) of 22.53 cm2/Vs, a high Ion/Ioff of ∼107, a low threshold voltage (Vth) of 0.15 V, and a minimum subthreshold swing (SS) of 0.24 V/decade. Furthermore, the threshold voltage shifts (ΔVth) in TFTs annealed in N2 and O2 are 0.31 and 0.16 V, respectively. These enhancements are attributed to the defects suppression and remaining ionized oxygen vacancies result in increased electron concentration in N2-annealed films. In comparison, O2 annealing causes a reduction in field effect mobility but concurrently enhances stability due to the direct passivation of defects, which leads to fewer oxygen vacancies. Additionally, Hf content can also impact the performance of TFT devices, even a small addition of Hf also results in the effective reduction of the carrier concentration. These findings provide valuable insights into the device mechanism of IHZO TFTs, presenting a novel avenue for comprehending and augmenting their overall performance.
Published Version
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have