AbstractSilica‐containing polyimide films were prepared by sol‐gel technique using a poly(amic acid) and tetraethoxysilane. The poly(amic acid) was synthesized by solution polycondensation reaction of 4,4′‐oxydiphthalic anhydride with 2,6‐bis(3‐aminophenoxy)benzene and an aminosilane coupling agent, 3‐aminopropyltriethoxysilane. The properties of these films, such as water vapors sorption capacity, dynamic contact angles and contact angle hysteresis, thermal, and electrical behavior have been evaluated with respect to their structure. The polymer films exhibited good thermal stability having the initial decomposition temperature above 450°C, glass transition temperature in the range of 223−228°C, and low‐dielectric constant in the range of 2.64−3.16. Two subglass transitions, γ and β, were evidenced by dynamic mechanical analysis and dielectric spectroscopy. The surface morphology and the roughness were investigated by atomic force microscopy and scanning electron microscopy. POLYM. ENG. SCI., 2010. © 2009 Society of Plastics Engineers

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.