Abstract

Coupled with hot-continuous rolling technology and based on the calculation of the finishing rolling impact work in the non-quenched and tempered Si-Mn steel, the calculations of the finishing rolling impact work in the alloying non-quenched and tempered steel with the elements of Cr, Ni, Mo, W, Cu, V, Nb and Ti are studied with the covalent electron number nA of the strongest bond in alloying phases, the smallest electron density difference Δρ of phase interfaces, and the number of atom states σ(σ’) which keep the interface electron density continuous. The calculated results show that the finishing rolling impact work of the alloying non-quenched and tempered steel intensely depends on strengthening mechanisms. The solution strengthening, interface strengthening, precipitation strengthening of pearlite, and dispersion strengthening will result in the decrease of the finishing rolling impact work; the refinement strengthening, the precipitation strengthening of V, Nb and Ti in α-Fe-C-V(Nb, Ti), and the residual austenite containing Ni on the boundary of α-Fe-C-Ni will increase the impact work; and the increments or decrements can be calculated with nA, Δρ, σ(σ’) and weights of alloying elements. The calculation formulas of the finishing rolling impact work in this paper are intergraded with the suggested ones of the finishing rolling tensile strength, yield strength, and elongation of the non-quenched and tempered steel. The calculated results agree well with the measured ones.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call