Abstract

The surface energies of solid molybdenum, niobium, tantalum, and tungsten at 1500 °C have been determined using the multi-phase equilibration technique. The values obtained were 2050, 2550, 2680 and 2830 erg/cm 2, respectively. The grain boundary energy/surface energy ratios for the four metals varied from 0.28 to 0.38 with an average of 0.32.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.