Abstract

The Strength of the Adhesive Joints of the Medium-Density Fireboards and Particle Boards with the PVC Film

Highlights

  • The bonding technology enables to obtain the high-quality adhesive joints that are characterised by high strength and resistance to the extrinsic factors [1,2,3,4,5]

  • The following conclusions may be drawn: 1. The adhesive joints made of the particle board with pressed 0.3 mm thick PVC film and the adhesive’s basis weight of 24 g/m2 are characterised by better strength properties than the adhesive joints of the particle board with the adhesive’s basis weight of 48 g/m2

  • The adhesive joints made of the particle board with pressed 0.8 mm thick acrylic film and the adhesive’s basis weight of 48 g/m2 are characterised by better strength properties than the adhesive joints with the adhesive’s basis weight of 24 g/m2

Read more

Summary

Introduction

The bonding technology enables to obtain the high-quality adhesive joints that are characterised by high strength and resistance to the extrinsic factors [1,2,3,4,5]. Bonding is used for bond the wooden elements, as well as to create various layer structures that are subject to further processing and that may be bonded with use of the bonding method later on. Such structures include various types of the furniture boards [15,16,17,18], e.g. particle board and MDF, which are used for production of either whole furniture constructions or their pieces. They are made of various particles that are arranged in a disordered manner [19]

Objectives
Methods
Results
Conclusion
Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call