Abstract

The concept using an off-axis filler wire during laser welding is introduced here in order to provide added process robustness considering gap width variations. Its stability is investigated with respect to gap width, welding speeds and powers. Geometry of the welds is analysed by tracing of weld cap edges and joint cross sections, connecting trends to weld parameters. High speed imaging and streak images are used to further study and describe sequences of events, including undercut formation. Formation of imperfections are found to be mainly correlated to wire feed position variations at the surface due to irregular melting of the wire tip.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.