One promising way of compensating for the repeated volume expansion and contraction of silicon as an anode active material in lithium ion batteries (LIBs) is to embed silicon within a graphite matrix. Silicon-graphite (SiG) composites combine the advantageous properties of graphite, i.e., large electrical conductivity and high structural stability, with the advantageous properties of silicon, i.e., high theoretical capacity. Graphite has a much lower volume expansion upon lithiation (≈ 10%) than pure silicon (≈ 300%) and provides a mechanically stable matrix. Herein, we present an investigation into the electrochemical performance and thickness change behavior of porous SiG anode compositions with silicon contents ranging from 0 wt% to 20 wt%. The electrode composites were studied using two methods: in situ dilatometry for the thickness change investigation and conventional coin cells for the assessment of electrochemical performance. The measurements show that the initial thickness change of SiG electrodes increased significantly with the silicon content, but it leveled off during cycling for all compositions. There appears to be a correlation between silicon content and capacity loss, but no clear correlation between thickness change and capacity loss rate was found.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.