Abstract

Low temperature hermetic wafer bonding using In/Sn interlayer and Au/Ni/Cu metallization as the high-melting-point (HMP) components was reported, wherein the thin Ni layer was introduced as a buffer layer to prevent solder consumption after their deposition. 8 in. wafer to wafer bonding was achieved at 180 °C for 20 min under 5.5 Mpa. Voids free seal joints composed of high temperature intermetallic compounds were obtained with good hermeticity. Present results show that the buffer layer is the key to ensure high yield hermetic wafer bonding when the low-melting-point solder was deposited directly on the HMP component.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.