Abstract

The ZnO:N films are prepared by a wet chemical method. The temperature-dependent photoluminescence (PL) is used to investigate those ZnO: N films. Due to the introduction of nitrogen atoms into ZnO film, another phase appears in the ZnO film, which can release the stress and improve the film quality. As a result, a neutral donor-bound exciton (D0X) emission peak is shown in low temperature PL spectrum. With the increasing temperature, the D0X line gradually loses its intensity and shifts to 3.30 eV, which is consistent with the well-known conversion from bound exciton to free exciton at elevated temperatures. Then, due to the thermal quenching effect, the D0X line vanishes in room temperature. In addition, no shift is shown in the location of visible band emission and only the intensity decreases with the increasing temperature.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.