Abstract

The main objective of this work was to assess the optimization of Fe and Cu bioleaching from converter slag using Acidithiobacillus ferrooxidans. Important parameters that contribute to the bioleaching process include initial pH, initial Fe2+ concentration and pulp density. In order to optimize these parameters, the response surface methodology (RSM) was applied. The maximum simultaneous Fe and Cu recovery yields were 95% and 100%, respectively. The optimum conditions were initial pH 1.8, initial density 1.4 g/100 mL and initial Fe2+ 7.3 g/L. The comparison between chemical leaching and bioleaching results showed that bioleaching improved the recovery yields of Fe and Cu by 26% and 33%, respectively. The modified shrinking core model was used to determine the rate-limiting step of the process. It was found that diffusion through the product layer and chemical reaction are the rate controlling steps.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.