Abstract

Thin films of CdS have been prepared on glass substrates by the chemical spray pyrolysis method at 250oC from solutions including different concentrations of Na2S (0.2 g and 0.4 g). The films were examined using SEM, an X-ray spectrometer, and a UV-Visible spectrometer. The SEM images and X-ray spectrum show that the films were amorphous, and the grain size varied with Na2S concentration. The optical properties and optical constants also varied clearly with Na2S concentration; in addition, the energy gap changed from 2.3 eV to 2.4 eV for both films.