An analysis of the influence of certain technological factors on the synthesis and sintering processes of spinel with excess periclase showed that spinel formation from various starting materials is largely complete at 1500°C. Firing at 1650–1750°C results in complete synthesis and approximately equal densities with various magnesite components. It was shown that waste materials from the production of abrasives can be used in place of commercial alumina.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.