The outcome of cryogenic treatment (CTT) on the mechanical behaviour of Al alloy LM 25, LM25+5% fly ash and LM25+10%fly ash composites was investigated. Cryogenic treatments were performed with threedifferent soaking periods (0 hr (Untreated), 12hr, 24hr) ata constant cryogenic temperature of -196°C. After the CTT, the mechanical behaviour of the materials was measured. It is obvious that LM25+10% fly ash composites exhibitbetter mechanical properties than the LM25 and LM25+10% fly ash composites.As cryogenic soaking period increases mechanical properties of the MMCs tend to increase too. The effect of fly ash mass percentage and cryogenic soaking period on the mechanical behaviour of materials was studied by using Taguchi and Analysis of Variance (ANOVA).
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
More From: International Journal of Innovative Technology and Exploring Engineering
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.