Abstract

We consider the features of formation of AuTiPd ohmic contacts to p + -Si. Metallization was made by vacuum thermal sputtering of Pd, Ti and Au films onto the Si substrate heated up to 330 С. It is shown that the contact resistivity increases with temperature; this is typical of metallic conductivity. We suggest that the ohmic contact is formed owing to appearance of shunts at Pd deposition on dislocations or other structural defects. The number of shunts per unit area is close to the measured density of structural defects at the metalSi interface. + -Si.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.