Barium Titanate (BT) has been synthesized using solid-state reaction method. Raw materials are Barium Carbonate (BaCO3) and Titanium Dioxide (TiO2). These materials are mixed for 6 h and sintered at a temperature of 1000oC, 1100oC, and 1200oC for 2 h. The sintering temperature was varied to investigate its effects on microstructure and dielectric constant of BT. The XRD patterns showed that BT becomes homogenous, with the large lattice parameter as the increase of sintering temperature. The crystal structure of BT is tetragonal. The crystalline size and crystallinity of BT at a sintering temperature of 1000oC are 37 nm and 97%. Those values for BT at a sintering temperature of 1100oC are 38 nm and 96%. At a sintering temperature of 1200oC, the values are 41 nm and 97%. The dielectric constant of BT at a sintering temperature of 1000oC, 1100oC, and 1200oC are 148, 163, and 185, respectively. It can be concluded that sintering temperature affects microstructure and dielectric constant of BT. High sintering temperature produces a high dielectric constant of BT. It indicates that crystalline size increases.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.