Abstract
The effects of adding small amounts ofMg to Ni- Cr-Mo-Ti-Nb and Ni-Cr- W-Mo-Al-Ti Ni-base superalloys on the stress rupture lives have been studied. The features ofvarious precipitates at the grain...
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.