ZnO–B2O3–SiO2 additive with 0.55: 0.35: 0.10 molar ratio was added to Ba0.3Sr0.7TiO3 ceramics in order to lower the sintering temperature. The densification behavior, crystalline structure, microstructure, dielectric properties and breakdown strength of ceramics were studied. When 9 wt.% additive was mixed with pure Ba0.3Sr0.7TiO3 powder, the densification temperature of samples decreased from 1350°C to 1100°C compared with no additive system, and the sintered ceramics revealed dielectric properties at room temperature as follows: dielectric constant ϵr = 413, dielectric loss tanδ = 0.00231 under 1 kHz and the breakdown strength Eb = 9.2 kV/mm.