Abstract

Pure aluminum wires of 9.25 mm diameter have been drawn at room temperature up to a true wire drawing strain of 2.09 at four different speeds (139.7, 84.7, 42.3 and 16.9 mm s −1). The yield strengths of these drawn wires indicate alternate hardening and softening during wire drawing and are insensitive to wire drawing speeds. The cell sizes are also not affected by the wire drawing speeds even though they decrease with increase in true wire drawing strain.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.