Abstract

The utilization of fly ash with low alumina has been carried out. The addition of TiO2 to the base material of fly ash and fly ash added with 20% metakaolin mixed with an alkaline solution has been characterized by heat resistance, compressive strength and porosity. These results indicate that the addition of TiO2 to both fly ash and fly ash with an additional 20% metakaolin shows a reduction in porosity reduction, an increase in the compressive strength value, and an increase in the thermal resistance of the sample. Despite an increase in the compressive strength value, however, the minimum requirement for a fire brick has not been achieved.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.