Abstract
A set of polystyrenes of comparable molecular weight around 4000, prepared by anionic polymerisation, were end-capped with various structures. Their thermal degradation behaviour (weight loss kinetics, nature and amount of volatile by-products) is governed by the nature of the chain ends. Some features of the degradation mechanisms are discussed.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.