Abstract
Dissimilar lap joint between aluminum 6061 and brass is performed by using friction stir welding (FSW) method where universal milling machine is used to implement this method. The parameters that use in welding are probe design with a varied length of pin probe 11.0 mm, 11.5 mm and 12.0 mm at 2000 rpm rotation of machine and feedrate 10 mm min−1. The macrostructure result of pin probe length 11.0 mm better than of pin probe 11.5 mm and 12.0 mm. The mechanical properties results with a pin probe length 11.5 mm a higher mean hardness value of 104.26 VHN than a pin probe length 11.0 mm and 12.0 mm with hardness values of 98.93 VHN and 70.43 VHN. Shear stress result of 67.32 MPa with a pin probe length 12 mm, better than of pin probe length 11.0 mm and 11.5 mm shear values of 40.2 MPa and 42.14 MPa.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
More From: IOP Conference Series: Materials Science and Engineering
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.