The purpose of this study was to evaluate histologically the effect of LiF-maleic acid added calcium aluminate (LM-CA) bone cement and calcium aluminate-polymethylmethacrylate (CA-PMMA) composite bone cement on bone regeneration in rat calvarial defect. After calvarial defects in 8 mm in diameter were created, three groups of 10 animals, a total of 30, each either received LM-CA bone cement, CA-PMMA composite bone cement or a sham-surgery control. Histologic analysis was done at 2 weeks and 8 weeks of healing periods. We concluded that LM-CA bone cement can be used as a bioactive bone graft material due to ability of bonding to the existing bone and CA-PMMA can be used as a graft material for augmentation of bone-volume due to dimensional stability.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.