ObjectiveThis study aimed to assess the effect of different storage media on the hardness and monomer elution of CAD/CAM composite blocks. MethodsFive resin-composite blocks (RCB), one polymer-infiltrated ceramic network (PICN) block (Enamic (EN)), one ceramic-filled poly ether ether ketone (PEEK) block (Dentokeep (DK)), and one feldspathic ceramic block. Microhardness was measured using a Vickers indenter tester (FM-700, Future Tech Corp., Japan). In addition 4 conventional resin-composites were investigated for monomer elution using high performance liquid chromatography (HPLC) after storage in different media for 3 months. The data were analysed by three-way ANOVA, two-way ANOVA, one-way ANOVA, Tukey’s post hoc test and the independent t-test (α=0.05 for all tests). ResultsThe specimens stored in the water had a hardness reduction ranging from 0.9% to 24.4%. In artificial saliva, the specimens had a hardness reduction ranging from 2.8% to 23.2%. The hardness reduction percentage in 75% Ethanol/Water (E/W) ranged between 3.8% and 35.3%. All materials, except GR (resin-composite block) and DK (Polyetheretherketone (PEEK)), showed a variable extent of monomer elution into 75% E/W with significantly higher amounts eluted from conventional composites. GRA and GND (conventional resin-composites) eluted TEGDMA in artificial saliva and GRA eluted TEGDMA in water. SignificanceThe hardness of CAD/CAM composite blocks was affected by different storage media, and they were not as stable as ceramic, with PICN exhibited superior hardness stability to all of the resin-composite blocks in all the storage media and was comparable to ceramic block. The hardness reduction percentage of the CAD/CAM composite blocks was influenced by the filler loading and resin-matrix composition.Minimal or no monomer elution from CAD/CAM blocks was detected.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call