Abstract

The effect of C content on the decomposition temperature of Bi 2Sr 2CaCu 2O 8 (Bi2212) with 0 and 10 wt.% added was investigated in atmospheres of 0.01,and 0.21 and 1.00 bar oxygen. The C content of the samples was controlled by a high-temperature heat treatment and subsequent exposure to H 2O saturated air. It was found that an increase in C content from 30 ppm to 7000 ppm suppressed the decomposition temperature of Bi2212 by only 3°C independent of Ag content. Furthermore, it was found that the previously observed suppression of the decomposition temperature with the addition of Ag was unaffected by changes in the C concentration from 80 to 1500 ppm.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.