Abstract

AbstractThe interfacial adhesion of blend of isotactic polypropylene/poly(vinyl methylether) (i‐PP/PVME) has been improved by the addition of poly(propylene‐g‐acrylic acid) (PP‐g‐AA) as a compatibilizing agent. The phase morphologies of the blends are investigated by optical microscopy (OM) and lateral force microscopy (LFM). The i‐PP/PVME (80/20) blend with no addition of PP‐g‐AA from extrusion process shows a coarse morphology with the dispersed domain size as large as several micrometers; After the addition of 2.5% PP‐g‐AA in the blends, the dispersed PVME domain size decreases greatly. The addition of 5% PP‐g‐AA results in a homogeneous morphology. The blending of PP‐g‐AA with PVME reduces the crystallization temperature of PP‐g‐AA, which is different from that of blending i‐PP with PVME. The increase of the interfacial adhesion is attributed to the specific intermolecular interaction between the acrylic acid group of PP‐g‐AA and the ether group of PVME. The specific interaction is studied by Fourier transform infrared spectroscopy. © 2006 Wiley Periodicals, Inc. J Appl Polym Sci 101: 4098–4103, 2006

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.