Abstract

In this study, with a view to improve the mechanical properties, the influence of the change in the micro-structure, crystal phase and mechanical properties were evaluated, by changing the amount of one of the sintering additives, Al2O3 and the HIP sintering conditions, from the viewpoint of the micro-structure consisting of α-Si3N4, β-Si3N4 and glassy grain boundary phase. The experimental results showed that 1) the combination of the sintering additives makes a various sorts of crystals and glassy phase formed which promotes the densification, 2) the addition of Al2O3 was effective in the densification, further, 3) as for the HIP sintering condition, N2 gas pressure higher than 60MPa greatly influences the transformation from α-Si3N4 to β-Si3N4 with densification. Si3N4 ceramics consist of both α-Si3N4 and β-Si3N4 crystal phase has been applied to various applications for industrial wear parts, instead of metals and cemented carbides which have been applied already.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.