Color stability is one of the denture base material requirement. Nowadays, nylon thermoplastic resin and heat-cured acrylic resin which is used as denture base materials can be changed in colour. One of a colour-changed factor is the tea drinking habit. The objective of this research was to compare the colour stability between nylon thermoplastic resin and heat-cured acrylic resin after soaked in tea. Materials used for the research were nylon thermoplastic resin from Valplast and heat-cured acrylic resin QC-20, with a sample size of 64x(10±0.03)x(2.5±0.03)mm. The sample would be assessed of colour stability after the denture base soaked in tea for 7 days. The colour measurement of each sample was done by spectrophotometer equipment (CIE lab system). Data gathered later on statistically processed with ANOVA testing. The result showed that the comparison ratio of colour stability between nylon thermoplastic resin and heat-cured acrylic resin after soaked in tea was 1.9886:1.1152. The conclusion was that colour stability in the nylon thermoplastic resin was lower than heat-cured acrylic resin after soaked in tea. This result was due to a polymer chain of nylon thermoplastic which was lower than heat-cured acrylic resin and its porosity which was higher, so tea easily soaked into the materials.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.