An experimental investigation of structure evolution kinetics in a new six-component TiAl-based alloy Ti-44.5Al-2V-1Nb-(0.5…L5)Zr/(L5…2.5)Cr-(0…0.1Gd) (at.%) with variable Zr, Cr, and Gd content has been accomplished under the conditions of high-temperature exposures in the temperature range 1000–1300°C and durations of 15–240 min. The Temperature – Time – Transformation diagrams have been constructed to summarize data on isothermal phase transformations for both Zr(+Gd)- and Cr(+Gd)-containing compositions with the initial as-cast structure. It is shown that the variation of Zr and Cr contents within the given limits for the studied alloy, as well as the doping with Gd microadditions in the amount of 0.1 at.% do not lead to any noticeable effect on the kinetics of structure behavior in isothermal conditions.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
More From: IOP Conference Series: Materials Science and Engineering
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.