Abstract

Influence of thermal annealing as a function of temperature and time, on magnetic and structural properties of Fe78Si3.6Cl3.4Mn0.65B4.35 (Fe78Si3.6Cl3.4Mn0.65 = Ci) alloy has been reported. Information on structure, formed nano-crystalline phases and their correlation with magnetic properties has been studied using, magnetic measurements, differential scanning calorimetery (DSC) and x-ray diffraction (XRD). Thermal annealing treatment leads to rather coarse grain microstructure (∼31 nm) accompanied by surface crystallization that appears to deteriorate the magnetic properties with annealing temperature.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.