ABSTRACTThin hydrogenated amorphous silicon carbide (a-SiC:H) films were grown at substrate temperatures ranging from 200 K to 600 K by remote ECR plasma-enhanced CVD. Mono- and trimethylsilane were used as single source precursors. The films grown using both precursors were compared as a function of temperature by in situ multiple internal reflection Fourier transform infrared (MIR-FTIR) spectroscopy. The difference in growth temperature leads to changes in both the hydrogen content and the composition of the film. At low growth temperature, films incorporate high concentrations of intact methyl group and a mixture of SiHx (x=1–3) groups, with a polysilane-like structure. At higher temperatures, the hydrogen content decreases. This decrease is observed in two different ways: (1) a loss of highly hydrogenated SiHx groups (SiH3 or SiH2); and (2) a shift from methyl groups to CH2 and CH bonding. However, the temperature dependence of each functional group is found to be different for the two precursors.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.