Abstract

The superconducting Bi 2Sr 2CaCu 2O 8+ x (Bi-2212) phase has been deposited by halide CVD on two different substrate materials, MgO(001) and SrTiO 3(001). Metal iodides and oxygen were used as precursors. The films grew with a strong [001] orientation and only the 00 l reflections with l=2 n were observed. The in-plane orientational relationships were determined by TEM to be [100] MgO//[100] Bi-2212 and [100] MgO//[110] Bi-2212 for the MgO(001) substrate and [100] SrTiO3//[110] Bi-2212 for the SrTiO 3(001) substrate. The interfacial regions of the two substrate materials were investigated by cross sectional HREM, revealing that the interface is nearly atomically abrupt for both substrate materials. The first atomic layer of the films were found to be a BiO layer.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.