Abstract

Tungsten nanopowders were synthesized by a chemical metallurgy method at 440–640 °C from WO3 precursors possessing different specific surfaces. The α-W nanopowder synthesized at 640 °C was not pyrophoric, while the α-W containing the traces of oxides obtained at 480 °C was pyrophoric. The temperature interval for the α-W synthesis was revealed as very narrow, from 470 to 490 °C.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.