AbstractIn this study, porous amorphous SiO2−Al2O3 (ASA(Si/Al=x)) with different Si/Al ratios was synthesized by gel‐gel method, and used to catalyze green renewable energy source γ‐valerolactone (GVL) to butene. Research indicated that all prepared catalysts had large amounts of disordered mesoporous with the pore size in range of 2–13 nm. For the optimal ASA(Si/Al=20) catalyst, its specific surface area is 430.20 m2 g−l and pore size is about 8.13 nm. Due to the presence of suitable Al species, ASA(Si/Al=20) has the largest Brønsted/Lewis ratio and 0.5554 mmol g−1 weak acid site content. Under the optimized reaction conditions, 90 % butene yield can be obtained in 180 min at 300 °C. In addition, the regeneration performance of the ASA(Si/Al=20) catalyst is also satisfactory, and the yield of butene can be above 60 % after 5th cycles. After activation, the spent catalyst can be regenerated, and about 78 % butene yield can be also obtained.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call