Abstract
Synthesis of LaYO3 was carried out via conventional solid state reaction method. The polycrystalline samples were sintered at temperatures in the range of 1300 °C to 1500 °C with each deviation is 50 °C. X-ray diffraction (XRD) analysis indicated that the perovskite ceramic obtained its single phase at 1500 °C with ordered monoclinic perovskite structure. The pure phase sample showed 98.79 % relative density and scanning electron micrographs also proved that the porosity of the sample reduced when sample undergo sintering.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.