Abstract

A novel five-step method for fabricating mesoporous SiO 2 glass was described in this paper, which consists of: (1) formation of colloidal suspension of Zn(OH) 2, (2) synthesis of silica sol, (3) mixture of Zn(OH) 2 colloidal suspension and silica sol to form nano-ZnO embedded precursor glass, (4) annealing of the precursor glass, and (5) treating nano-ZnO embedded glass with HCl to obtain the mesoporous glass. The mesostructure of the glass was investigated by X-ray diffraction (XRD), field emission scanning electron microscope (SEM), and BET surface area analysis. The average pore size distribution is in the range of 3.7 nm, and the surface area is as high as 496.5 m 2/g.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.