Abstract

AbstractPolyether polyols can improve the performance of waterborne epoxy curing agent. In this paper, intermediates were synthesized from polyether triols with epoxy resin E‐51 and introduced into the epoxy curing agent by reacting with TETA. This paper focuses on the process of synthesizing the intermediates. The 2K waterborne epoxy coating film prepared with polyether triols‐modified waterborne epoxy curing agent exhibits desirable corrosion protection capacity and neutral salt spray resistance up to 600 h. In addition, the 2K waterborne epoxy coating film prepared using the modified waterborne epoxy curing agent with polyether triols displayed improved surface appearance, mechanical properties, and water resistance.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.