Abstract

“Living” poly(methyl methacrylate) (PMMA), prepared by the RAFT technique, reacted with maleic anhydride to give succinic anhydride-terminated PMMA (SA−PMMA) in very high yield. The ω-terminal anhydride residues react in high yields with primary alcohols, primary amines and aromatic amines. As examples, SA−PMMA reacted with 1H,1H,2H,2H-perfluorodecylamine to give a polymer containing 5.78% of fluorine; with Disperse Orange 3 to give a dye-labeled PMMA; with 9-hydroxymethylanthracene to give a fluorescently labeled PMMA; with norephedrine to give a polymer with a biologically active end group; and with 4,4′-diaminophenymethane to give amine-ended PMMA. The latter reacted smoothly with fluorescein isocyanate to give a fluorescently labeled PMMA. In these examples the fraction of polymer chains functionalized were in the range 75−95%. Allowing for the fact the starting PMMAs were up to 96% “living”, these loadings correspond to functionalization yields, for the anhydride addition plus the reaction with the n...

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.