Graft copolymers of poly(methyl methacrylate) with poly(3-hydroxybutyrate), PHB, segments as long side chains were prepared by the macromonomer method. PHB macromonomers were prepared from the esterification of oligomers with 2-hydroxyethyl methacrylate at their carboxylic acid end. Esterification products displayed low polydispersity indices (ca. 1.2) and a functionality of over 83%, with a Mn of 2,020. Using free radical polymerization methods, the macromonomers were copolymerized with methyl methacrylate to yield graft (comb type) copolymers at different comonomer feed ratios. The graft copolymers contained from 0.5 to 14 mol-% of PHB blocks, with a glass transition temperature decreasing from 100 to 3 degrees C.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.