Abstract

A novel monomer of tetrachloroterephthaloyl chloride (TCTPC) was prepared by the chlorination of terephthaloyl chloride catalyzed by ferric chloride at 175–180°C for 10 h and confirmed by FTIR, MS, and elemental analysis. Five new polychloro substituted poly(aryl ether ketone sulfone)s (PEKSs) with inherent viscosities of 0.68–0.75 dL/g have been prepared from 4,4′-diphenoxydiphenylsulfone, 4,4′-bis(2-methylphenoxy) diphenylsulfone, 4,4′-bis(3-methylph-enoxy)diphenylsulfone, 4,4′-bis(2,6-dimethylphenoxy)diphenylsulfone, and 4,4′-bis(1-naphthoxy)-diphenylsulfone with TCTPC by electrophilic Friedel-Crafts acylation in the presence of DMF with anhydrous AlCl3 as a catalyst in 1,2-dichloroethane, respectively. These polymers having weight–average molecular weight in the range of 76,600–83,900 are all amorphous and show high glass transition temperatures ranging from 213 to 250°C, the 5% weight loss temperature over 450°C, high char yields of 60–67% at 700°C in nitrogen and good solubility in CHCl3 and polar solvents such as DMF, DMSO, and NMP at room temperature. All the polymers formed transparent, strong, and flexible films, with tensile strengths of 85.1–90.8 MPa, Young's moduli of 2.52–3.24 GPa, and elongations at break of 21.2–27.2%. © 2008 Wiley Periodicals, Inc. J Appl Polym Sci, 2008

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.