AbstractA new polymer‐forming monomer, 3,4‐bis(4‐aminophenyl)‐2,5‐diphenylpyrrole, was synthesized in three steps starting from 4′‐nitrodeoxybenzoin. Tetraphenylpyrrole‐containing aromatic polyamides and copolyamides were prepared from the diamine with various aromatic diacid chlorides and from a mixture of the diamine and 4,4′‐oxydianiline with terephthaloyl chloride, respectively. The resultant polymers had inherent viscosities in the 0.3–1.8 dL/g range and were generally soluble in various organic solvents including N,N‐dimethylacetamide and m‐cresol. They have glass transition temperatures in the range of 306–333°C and showed no weight loss below 380°C in both air and nitrogen atmospheres.