Abstract

AbstractNovel, soluble aromatic polyamides and copolyamides containing tetraphenylethylene units were prepared by the low temperature solution polycondensation of 1,1‐bis(4‐aminophenyl)‐2,2‐diphenylethylene and aromatic diamines with various aromatic diacid chlorides. Highmolecular‐weight polyamides having inherent viscosities of 0.6–1.5 dL/g and number‐average molecular weight above 21000 were obtained quantitatively. These polymers were readily soluble in various solvents such as N‐methyl‐2‐pyrrolidone, N,N‐dimethylacetamide (DMAc), and dimethyl sulfoxide and gave pale yellow, transparent, flexible films by casting from DMAc solution. The polymers had glass transition temperatures between 290 and 340°C, and started to lose weight around 400°C, with 10% weight loss being recorded at about 470°C in air.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.