Finely dispersed (CeO2)0.95(Sm2O3)0.05, (CeO2)0.90(Sm2O3)0.10 and (CeO2)0.80(Sm2O3)0.20 mesoporous powders with a specific pore volume of 0.080–0.092 cm3/g and a specific surface of 50–83 m2/g are synthesized by the co-precipitation of cerium and samarium hydroxides from the corresponding nitrate solutions. The prepared powders are used to obtain ceramic nanomaterials with a fluorite-like cubic crystal lattice with a coherent scattering region (CSR) of about 65–69 nm (1300 °C). The study of physicochemical and electrophysical properties of the prepared ceramics revealed the obtained materials featuring an open porosity of 2–6% and a predominantly ionic type of electric conductivity (ion transport numbers ti = 0.85–0.73 in the temperature range 300–700 °C). The conductivity in solid solutions proceeds via a vacancy mechanism with σ700 °C= 3.3·10−2 S/cm. The synthesized ceramic materials are shown to be promising as solid oxide electrolytes in medium temperature fuel cells.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.