Bi 2S 3 nanorods were synthesized via a simple solvothermal process in polyol media through the reaction between Bi(NO 3) 3·5H 2O, urea and CS 2 at 150 °C for 15 h using diethylene glycol as solvent. The nanorods were characterized by XRD, TEM and SAED. The results showed that the products were well-crystallized orthorhombic phase with lattice parameters a = 11.15 Å, b = 11.3 Å and c = 3.984 Å, which are consistent with the value in standard JCPDS card No. 17-0320. DEG served as an excellent solvent and structure director. Besides, compared to water and EG as solvents, the DEG system can provide a mild and homogenous condition, which is favorable to anisotropic growth and increases the yield of high quality Bi 2S 3 nanorods. Based on the experimental results, the growth mechanism was discussed.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.