Abstract
Materials including Cu2Se, Cu2Se0.96−xSxTe0.04 (x = 0.00–0.03) and Cu2−ySe0.94S0.02Te0.04 (y = 0.00–0.04) were synthesized using aqueous solution processing at room temperature and cold-press sintered under vacuum at 650 °C for 6 hours.