Abstract
A pulsed XeCl excimer laser was used to deposit amorphous Nd‐modified lead zirconate titanate thin films with thicknesses between 25 and 500 nm. Atomic force microscopy was used to study the thin‐film surface morphology and to determine the particulate number density (PND) on film surfaces. The dependence of the PND and the growth rate of the film on the laser‐beam fluence and the density of Pb0.97Nd0.02(Zr0.55Ti0.45)O3 targets was also studied. It was found that the PND of particulates with diameters larger than 150 nm increased with increasing laser‐beam fluence and decreased with increasing target density. The surface morphology and quality of the target after ablation were studied by scanning electron microscopy. The generation of laser‐cone structures and particulates at the target surface was also studied. X‐ray diffraction measurements and element analyses by the energy dispersive spectroscopy of X‐rays revealed the formation of extra compounds and phases at the target surface during ablation processes. Raman spectroscopy was also used to study the structure of the topmost surface layer of the target after ablation.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.