Abstract

The surface morphology of low-energy Kr+-polished amorphous Si layers is studied by topographical methods as a function of initial substrate roughness. An analysis in terms of power spectral densities reveals that for spatial frequencies 2×10−2–2×10−3 nm−1, the layers that are deposited and subsequently ion polished reduce the initial substrate roughness to a rms value of 0.1 nm at the surface. In this system, the observed dominant term in linear surface relaxation, proportional to the spatial frequency, is likely to be caused by the combined processes of (a) ion-induced viscous flow and (b) annihilation of (subsurface) free volume during the ion-polishing treatment. Correspondingly, a modification of the generally assumed boundary conditions, which imply strict surface confinement of the ion-induced viscous flow mechanism, is proposed. Data on surface morphology are in agreement with the optical response in extreme ultraviolet from a full Mo/Si multilayered system deposited onto the modified substrates.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.