Abstract

Nanofiber scaffold has been widely developed as a tissue engineering material because it can imitate the ECM of bones. In this study, nanofiber scaffold is composed of polyvinyl alcohol (PVA), chitosan, polyethylene glycol (PEG), and hydroxyapatite (HAp) which have superior characteristics for tissue engineering applications. The nanofiber scaffold is synthesized using electrospinning. Experimental results show that dielectric barrier discharge (DBD) plasma treatment causes increased surface roughness, contributing to the improvement of surface wettability. This is indicated by a decrease in this contact angle from 9.92° to 1.74°. In addition, DBD plasma treatment also increased biodegradation as well as increased treatment time.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.