Abstract

An excellent modified polyester fiber was prepared via chemical grafting between polyester fiber and perfluorooctyltrimethoxysilane (FAS-17), or silane coupler (KH-570), or Titanate coupler (DN-101) in isopropyl alcohol aqueous solution. Volume ratio of isopropyl alcohol in aqueous solution was 50:50, the mass concentration of FAS-17 is 2%, reacting on polyester fiber modified for 24h at 60 °C, the polyester fiber contact angle to water was 145 °, and the contact angle to peanut oil was 118 °, with excellent performance of amphiphobic property. KH-570 and DN-101 modified polymer fiber to be hydrophobic properties nearly as FAS-17, but modified polyester fiber have no amphiphobic property.